	Group: Administrators 	        
    Posts: 2.5K, 
    Visits: 8.5K 
    
 
          
		     | 
				                       
                 
                
                    
			            We don't yet have any mechanical data for the woven finish tubes, although we are hoping to do some mechanical testing on them once our testing laboratory is fully set up and functional. 
  In terms of how much  strength will be lost, there is no easy way of knowing without either doing some tests or running an FEA simulation in CAD.                 
			            
  				
			            Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant                     
                     
                                            
                         
                    
                  
             |