By GreyArea - 12/6/2017 12:47:54 PM
I need to add some light transmisssion to a carbon fibre tube. Set of questions as follows;
What is the compressive strength of a 25mm CF tube along it’s axis? What is the flexural strength of a 25mm CF tube?
Now the harder questions;
If I were to drill 0.5mm holes in a triangular pattern at 1.5mm equidistant spacings for a third of the diameter (ie in a “strip” down one side of the tube, how much strength would I lose?
Thanks!
|
By GreyArea - 12/8/2017 2:38:37 AM
I thought that might be the case...oh well will just have to try it and see what happens.
|
|