In a couple of weeks, we are hoping to have our own UD pre-preg manufactured for us in stock. This is a Toray T700 based UD 300gsm fabric and comes on a 300mm wide roll. This is designed for autoclave use using the XC130 resin system seen in some of our other pre-pregs..
As soon as it is available, we will list it on the website and have further more specific details on cure cycle etc.
The picture you show looks like a picture of a raw UD fabric before it has been through the toll impregnation process which adds the resin, as it has no backing papers to stop it sticking together. You will also find different weavers use different methods to hold the UD together. Some use visble mesh fabrics or stitching, others use an internal net or mesh to hold it together.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|