Clearcoat Adhesion Problems


Author
Message
fgayford
fgayford
Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)
Group: Forum Members
Posts: 433, Visits: 1.2K
As I removed some tape from a piece of finished carbon fiber plate the Automotive clear coat peeled off like a sheet of plastic.
I have never been comfortable with the way I finish my products.

 What does your method look like?
What surface prep do you do before shooting the automotive clear coat? 
What is your final sanding grit?
What do you use for final wipe down?
Is there an adhesion promoter that is invisible in a clear finish?

I would really appreciate  hearing from you professionals.
Thanks
Fred