Clearcoat Adhesion Problems


Author
Message
Saff
Saff
Supreme Being (102 reputation)Supreme Being (102 reputation)Supreme Being (102 reputation)Supreme Being (102 reputation)Supreme Being (102 reputation)Supreme Being (102 reputation)Supreme Being (102 reputation)Supreme Being (102 reputation)Supreme Being (102 reputation)
Group: Forum Members
Posts: 10, Visits: 723
800 grit, degrease then 2k high solid clear coat, but I'm not a professional Smile


my facebook page
Interloper393
Interloper393
Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)
Group: Forum Members
Posts: 90, Visits: 634
I 400 grit sand. ,  clear coat wet sand with 800 then clear again
fgayford
fgayford
Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)
Group: Forum Members
Posts: 433, Visits: 1.2K
As I removed some tape from a piece of finished carbon fiber plate the Automotive clear coat peeled off like a sheet of plastic.
I have never been comfortable with the way I finish my products.

 What does your method look like?
What surface prep do you do before shooting the automotive clear coat? 
What is your final sanding grit?
What do you use for final wipe down?
Is there an adhesion promoter that is invisible in a clear finish?

I would really appreciate  hearing from you professionals.
Thanks
Fred