Concrete strong, stiff and light


Author
Message
scottracing
scottracing
Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
if you look for mould putty on the east composites forum thats what im on about.

The lamborghini forged composite is much  like cut up pieces of prepreg  but rather than being autoclave cured, they have a snap cure resin and are cured in tools in a heated press.



Rafael Chao
R
Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)
Group: Forum Members
Posts: 5, Visits: 17
Hi scottracing,

I thought forged composites was an option, but It looks like it needs injection molding, which makes the final product very expensive. I am looking for a paste like you said, curing period is not a problem, the point is to manufacture solid pieces with low costs.

Do you know exactly which tooling paste are you talking about? do yo know the name?

Thanks so much for your post


scottracing
scottracing
Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
Rafael Chao - 9/13/2017 3:45:38 PM
Hi Chris,

The link you added to your post talks about a paste of carbon fibers, mixed with a resine. It sounds pretty good, now I need to know if we need an oven, or we can you the paste directly on a mold without heating or something similar. Looks like it will need injection molds.

Next step is to find out who manufactures this forged Composites.

Thanks so much for your post !!!!

Easy composites sell a tooling paste made of glass fibres and epoxy resin. If you are looking for forged conposites like quantum conposites you will need a press or autoclave to cure and consolidate the material.
I think you are looking more for a paste that you can extrude?

Rafael Chao
R
Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)
Group: Forum Members
Posts: 5, Visits: 17
Hi Chris,

The link you added to your post talks about a paste of carbon fibers, mixed with a resine. It sounds pretty good, now I need to know if we need an oven, or we can you the paste directly on a mold without heating or something similar. Looks like it will need injection molds.

Next step is to find out who manufactures this forged Composites.

Thanks so much for your post !!!!

ChrisP
ChrisP
Supreme Being (123 reputation)Supreme Being (123 reputation)Supreme Being (123 reputation)Supreme Being (123 reputation)Supreme Being (123 reputation)Supreme Being (123 reputation)Supreme Being (123 reputation)Supreme Being (123 reputation)Supreme Being (123 reputation)
Group: Forum Members
Posts: 9, Visits: 281
Rafael Chao
R
Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)
Group: Forum Members
Posts: 5, Visits: 17
Rakesh Verma - 9/13/2017 9:22:30 AM
Rafael Chao - 9/13/2017 7:56:43 AM
Hi all,
I am looking for a pre preg or composite that allow me to create a "
paste" or semi-liquid, that once dried, with the next characteristics:

- Strong / stiffness similar to carbon fibre.
- Light / weight similar to aluminum.
I plan to create a mold (steel, aluminum...) and put this paste on it, dry it, and create strong, light solid pieces.
Do you provide this product?
Do you have a solution, composite, ingredients to obtain something similar?

Excellent website by the way.
Rafa

WE ARE THE MANUFACTURER OF AUTOCLAVE USED IN COMPOSITE INDUSTRY, CUSTOM MADE,
WE CAN MANUFACTURER AS PER ASME, CE, CRN, GOST, ISO9001 STANDARD
AS PER THE CUSTOMER REQUIREMENT
WE HAVE EXPORTED MORE THAN 32 COUNTRIES INCLUDING CANAD, EUROPE, ASIA, GULF, CUSTOMER ARE SATISFIED WITH OUR SERVICES AND QUALITY
Rakesh Verma (Overseas Manager)
rakesh@olymspan.com
+86-13861177443

Dear Mr. Verma,

As I said in my post, we want to manufacture solid pieces.

The pieces has to be strong, something similar to carbon fibre.
The pieces has to be light as well, something similar to aluminum….

The point here is that we don’t want to have a manual or complicated process. We consider working with carbon fibre complicated, because of the vacuum process, the manual process, etc…

We are looking for a process where we mix different products (like cooking), we can put some heat, not too much, and the liquid or paste produced with that mix, we will put it into standard molds. Once the mix is cured or dried, we open the mold, and we go for the next one.

Is that possible?

Thanks in advance,

Rafael Chao

Rafael Chao
R
Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)
Group: Forum Members
Posts: 5, Visits: 17
Rakesh Verma - 9/13/2017 9:22:30 AM
Rafael Chao - 9/13/2017 7:56:43 AM
Hi all,
I am looking for a pre preg or composite that allow me to create a "
paste" or semi-liquid, that once dried, with the next characteristics:

- Strong / stiffness similar to carbon fibre.
- Light / weight similar to aluminum.
I plan to create a mold (steel, aluminum...) and put this paste on it, dry it, and create strong, light solid pieces.
Do you provide this product?
Do you have a solution, composite, ingredients to obtain something similar?

Excellent website by the way.
Rafa

WE ARE THE MANUFACTURER OF AUTOCLAVE USED IN COMPOSITE INDUSTRY, CUSTOM MADE,
WE CAN MANUFACTURER AS PER ASME, CE, CRN, GOST, ISO9001 STANDARD
AS PER THE CUSTOMER REQUIREMENT
WE HAVE EXPORTED MORE THAN 32 COUNTRIES INCLUDING CANAD, EUROPE, ASIA, GULF, CUSTOMER ARE SATISFIED WITH OUR SERVICES AND QUALITY
Rakesh Verma (Overseas Manager)
rakesh@olymspan.com
+86-13861177443

Hi Rakesh, I have sent you an email.
Thanks for your answer.

Rafael Chao

Rafael Chao
R
Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)
Group: Forum Members
Posts: 5, Visits: 17
Hi all,
I am looking for a pre preg or composite that allow me to create a "
paste" or semi-liquid, that once dried, with the next characteristics:

- Strong / stiffness similar to carbon fibre.
- Light / weight similar to aluminum.
I plan to create a mold (steel, aluminum...) and put this paste on it, dry it, and create strong, light solid pieces.
Do you provide this product?
Do you have a solution, composite, ingredients to obtain something similar?

Excellent website by the way.
Rafa