thilina75
thilina75
posted 9 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 5,
Visits: 37
Hi ya,
I am an Aerospace Engineer working in a project, developing a electric super car and I am manufacturing car body panels using VARI process.
Recently I have came a cross some complecations with the panels that I have manufatured. (Please see the attcahed photos)
As you can see, there is a mist like marks in the corners for this front hood reinforced panel. I used gel coat on the mold.
Does anyone have any idea why I am getting these marks.
and any advise will be appriceated.
Kind regards.
Thilina.
Tags
VARI
Reply
Like
5
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Problems with VARI'd car body panels
thilina75
-
9 Years Ago
Can't quite see properly as I'm on my phone but it looks like fibre bridging and resin filling the...
FLD
-
9 Years Ago
It does look like bridging in those corners but a bit worse, maybe it has delaminated from the...
Warren (Staff)
-
9 Years Ago
looks like bridging to me especially in those tight rads where the material has scrunched up as you...
scottracing
-
9 Years Ago
Post Reply
Like
5
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search