question about making a mold for a car emblem


Author
Message
iarefluffy
iarefluffy
Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)
Group: Forum Members
Posts: 2, Visits: 28
not too sure how much time im suppose to wait between applying tooling and coupling coat. i waited about 2 hours or until slightly firm and slightly sticky, then put the fiberglass and coupling coat. Then when everything was dried after a day or so, removed my emblem and there were imprints from the fiberglass on it. Did i not leave enough time between the coats?