My first problem is "Mixing weights and Volume"


Author
Message
lenwatson
lenwatson
Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)
Group: Forum Members
Posts: 2, Visits: 23
The instructions for mixing the primer are to use 2% MEKP catalyst, the scales give weight in grams and mixing 75g of primer would require the scales to be accurate to half a gram to measure 1.5g. Is the percentage critical or would 2 grams be OK.
I thought the Catalyst bottle was the answer but it measures ml not grams so how much does 1ml of MEKP weigh?
Am I being confused or am I missing a trick?
I do not want to mix large amounts as I am making Brake cooling ducts for my race car and they are not big like a car hood/bonnet.