Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
New Member Introductions
»
My first problem is "Mixing weights and Volume"
My first problem is "Mixing weights and Volume"
Post Reply
Like
2
My first problem is "Mixing weights and Volume"
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
lenwatson
lenwatson
posted 8 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2,
Visits: 23
Thanks for that I will try to finish them today as we have a dyno test Thursday and the ducts fit behind the wheel bearings.
Reply
Like
2
Hanaldo
Hanaldo
posted 8 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
MEKP is so close to 1:1 that it is negligible, you can interchange weight for volume. So if you measured your resin by weight, it's no problem to measure your catalyst by volume.
Just be wary of using syringes for measuring catalyst. The catalyst can actually break down the rubber stopper and then contaminate your resin, causing all sorts of issues. It generally isn't a problem, but just something to be aware of. Better to use plastic pipettes for measuring small amounts.
Reply
Like
2
Fasta
Fasta
posted 8 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 468,
Visits: 3.5K
I usually go with the % as mls and I think that is the norm.
100g resin at 1% is 1ml.
If you are still worried about measurement of the catalyst then a small 5ml syringe can be more accurate than the regular catalyst dispensers.
Fastacraft Facebook page
Reply
Like
2
lenwatson
lenwatson
posted 8 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 2,
Visits: 23
The instructions for mixing the primer are to use 2% MEKP catalyst, the scales give weight in grams and mixing 75g of primer would require the scales to be accurate to half a gram to measure 1.5g. Is the percentage critical or would 2 grams be OK.
I thought the Catalyst bottle was the answer but it measures ml not grams so how much does 1ml of MEKP weigh?
Am I being confused or am I missing a trick?
I do not want to mix large amounts as I am making Brake cooling ducts for my race car and they are not big like a car hood/bonnet.
Tags
MEKP + primer mixing proportions
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search