Pin holes in laquar coats
Pin holes in laquar coats
Post Reply
Like
3
Pin holes in laquar coats
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Interloper393
Interloper393
posted 8 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 90,
Visits: 634
Hi guys iv skinned quite a few parts now, all have been sanded with 400 grit and there is no low spots or shiney spots so no pin holes and the piece us perfect...
Now I use upon 2k clear, I apply 4 light mist coats and wait 5 mins between coats, followed by a medium coat and a few heavy coats after 15 mins... so why am I getting pinholes in the cleat coat?
Iv waited 10 mins between coats and hit it with about 5 heavy coats and the dam things won't go away!
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Pin holes in laquar coats
Interloper393
-
8 Years Ago
Anyone? Need these parts away and ot ain't happening :(
Interloper393
-
8 Years Ago
Can you post photos? It will either be surface porosity or contamination.
Hanaldo
-
8 Years Ago
If you find you have visible pinholes on the surface, what you can do is wipe over the panel with...
Warren (Staff)
-
8 Years Ago
What would you use to wipe over the surface?
Interloper393
-
8 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search