Pin holes in laquar coats

http://www.talkcomposites.com/Topic22968.aspx

By Interloper393 - 3/19/2017 12:25:51 PM

Hi guys iv skinned quite a few parts now,  all have been sanded with 400 grit and there is no low spots or shiney spots so no pin holes and the piece us perfect...
Now I use upon 2k clear,  I apply 4 light mist coats and wait 5 mins between coats,  followed by a medium coat and a few heavy coats after 15 mins... so why am I getting pinholes in the cleat coat?  
Iv waited 10 mins between coats and hit it with about 5 heavy coats and the dam things won't go away! 
By Interloper393 - 3/20/2017 4:45:25 PM

What would you use to wipe over the surface?