If you find you have visible pinholes on the surface, what you can do is wipe over the panel with lacquer before spraying as it fills the pin holes with lacquer.
Otherwise with pinholes, the lacquer sprays over the top fine, all looks good, then as the solvents evaporate off and it cures, it sinks into the pinholes leaving dimples all over the lacquer.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|