Gave you a reply on composites central.

even that just touches the surface of the job
scottracing
scottracing
Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
If you are doing on the job repairs you want quick bonding stuff like wurth replast that cures in a couple of minutes. Prepreg work you will need a hot bonder ideally and snap cure resins. 
Neil1970
Neil1970
Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)
Group: Forum Members
Posts: 3, Visits: 200
Will be a combination of event support test and race and factory based I believe.
ajb100
ajb100
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
Do you have the mounds for them?
scottracing
scottracing
Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
its going to be dependent on if you are going prepreg or wetlay repair, you can get away with a decent scarfed wet lay repair in most instances. Or otherwise fill the damage then take a splash mould of the repaired section and lay up a new tool repair splash, lay into it and cut and bond the repair section into the panel.
Neil1970
Neil1970
Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)
Group: Forum Members
Posts: 3, Visits: 200
Making repairs to damaged body work so I'm after various options really 
scottracing
scottracing
Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
What kind of info are you after? Will you be replacing sections of bodypanels or repalcing and bonding.
Ive picked up myself a hot bonder recently for repair work with prepregs. But if youve worked with the materials before you should be fine.
Neil1970
Neil1970
Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)
Group: Forum Members
Posts: 3, Visits: 200
Hi there first posting on here but have previously worked with preg preg and wet lay for over 10 years but have been out of the game for a bit,has any one got any good info or no of any good links on carbon fibre repair could be doing some race car repair work soon many thanks.