By Neil1970 - 2/12/2017 12:54:56 PM

Hi there first posting on here but have previously worked with preg preg and wet lay for over 10 years but have been out of the game for a bit,has any one got any good info or no of any good links on carbon fibre repair could be doing some race car repair work soon many thanks.
By f1rob - 2/18/2017 2:22:04 PM

Gave you a reply on composites central.

even that just touches the surface of the job