Epoxy tooling gelcoat - use with polyester resin?
Epoxy tooling gelcoat - use with polyester resin?
Post Reply
Like
7
Epoxy tooling gelcoat - use with polyester resin?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Christian_83
Christian_83
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 5,
Visits: 70
Okay cheers mates.
Just hoped i could a corner with the polyester resin over epoxy resin lol. Funds are limited being back to school.
But no polyester for my epoxy gelcoat then.
Reply
Like
5
Hanaldo
Hanaldo
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
Yeh, definitely won't work. Even vinyl ester resin with an epoxy tooling gelcoat doesn't work in my experience.
Reply
Like
5
Fasta
Fasta
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 468,
Visits: 3.5K
It won't work, sorry.
It's a general no no to try and bond polyester resins to epoxy materials.
Fastacraft Facebook page
Edited
10 Years Ago by
Fasta
Reply
Like
5
Christian_83
Christian_83
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 5,
Visits: 70
Hi Guys.
Got some Epoxy tooling gelcoat for some small molds. I also bought some polyester resin and chopped mat.
Will the polyester resin work with the epoxy tooling gelcoat or will it only work with epoxy?
Cheers Christian
Reply
Like
7
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
7
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search