Hi Guys.
Got some Epoxy tooling gelcoat for some small molds. I also bought some polyester resin and chopped mat.
Will the polyester resin work with the epoxy tooling gelcoat or will it only work with epoxy?

Cheers Christian
Fasta
Fasta
Supreme Being (5.6K reputation)Supreme Being (5.6K reputation)Supreme Being (5.6K reputation)Supreme Being (5.6K reputation)Supreme Being (5.6K reputation)Supreme Being (5.6K reputation)Supreme Being (5.6K reputation)Supreme Being (5.6K reputation)Supreme Being (5.6K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
It won't work, sorry.

It's a general no no to try and bond polyester resins to epoxy materials.




Edited 10 Years Ago by Fasta
Hanaldo
Hanaldo
Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Yeh, definitely won't work. Even vinyl ester resin with an epoxy tooling gelcoat doesn't work in my experience. 
Christian_83
Christian_83
Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)
Group: Forum Members
Posts: 5, Visits: 70
Okay cheers mates.
Just hoped i could a corner with the polyester resin over epoxy resin lol. Funds are limited being back to school.
But no polyester for my epoxy gelcoat then.