Scout
Scout
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 6,
Visits: 19
Hi guys,
Just wanted to ask if I can use Addition Cure or CS25 Condensation Cure Silicone Rubber to create a "Vaccum bag" over a mould?
I was thinking if I could include the vaccum port/s into the mould flange itself and add a resin infusion port into this silicone rubber based vacuum bag would that work? Has anyone tried this?
Sorry guys might be a stupid question... but I thought I would ask
I am just a beginner but looking at the technical datasheet it looks like it can handle the pressure and the temperature?
Reply
Like
4
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Using Silicone Rubber for making vacuum bags
Scout
-
10 Years Ago
It would work for sure. If you use the addition cure silicone, then be aware that styrene inhibits...
Hanaldo
-
10 Years Ago
Thanks for the advise Hanaldo. I have watched the videos. I will give it a go. As for the...
Scout
-
10 Years Ago
[quote][b]Scout (21/10/2016)[/b][hr]Thanks for the advise Hanaldo. I have watched the videos. I will...
fgayford
-
10 Years Ago
Thanks Fred. I will watch their videos :)
Scout
-
10 Years Ago
I suspect not, but it's a good question. I would use something like a fibreglass scrim tape I think....
Hanaldo
-
10 Years Ago
Jeez, can't say I'm impressed by their infusion video, they just absolutely flood the laminate and...
Hanaldo
-
10 Years Ago
Post Reply
Like
4
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search