Hi guys,

Just wanted to ask if I can use Addition Cure or CS25 Condensation Cure Silicone Rubber to create a "Vaccum bag" over a mould?

I was thinking if I could include the vaccum port/s into the mould flange itself and add a resin infusion port into this silicone rubber based vacuum bag would that work? Has anyone tried this?

Sorry guys might be a stupid question... but I thought I would ask Smile I am just a beginner but looking at the technical datasheet it looks like it can handle the pressure and the temperature?
Reply
Scout
Scout
Forum Guru (58 reputation)Forum Guru (58 reputation)Forum Guru (58 reputation)Forum Guru (58 reputation)Forum Guru (58 reputation)Forum Guru (58 reputation)Forum Guru (58 reputation)Forum Guru (58 reputation)Forum Guru (58 reputation)
Group: Forum Members
Posts: 6, Visits: 19
Thanks Fred. I will watch their videos Smile
Edited 9 Years Ago by Scout
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search