Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Mould Making
»
advice on what release to use on pattern berfore laying up mould.
advice on what release to use on pattern berfore laying up mould.
Post Reply
Like
9
advice on what release to use on pattern berfore laying up mould.
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Porkster0
Porkster0
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 14,
Visits: 69
Hi all
I am new to mould making at home and to this site
I have a Uni-Mould kit from Easy Composites and have made a pattern for a kit car scoop using my original scoop from the car see picture attached
I would really like any tips / advice you may have on how to prep / release the pattern before making the mould
I have read instructions sheets and watch videos BUT would welcome any contributions as you cannot beat the experience of other people that have started out the same way
For example I have a block of filleting wax to use where there might be some under cuts but do i put this on before or after releasing the pattern
Thanks in advance for any helping a newbie
Regards
Ian
Attachments
scoop1.jpg
(
858 views,
433.00 KB
)
scoop2.jpg
(
866 views,
300.00 KB
)
Tags
dax rush
pattern
release
Edited
10 Years Ago by
Porkster0
Reply
Like
9
Reply
Fasta
Fasta
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 468,
Visits: 3.5K
Good job and excellent for the first effort.
Those damaged edges appear broken away from just getting caught when releasing. Just do a small gelcoat repair.
Dremmel/sand the broken area and just make a dam on one side with some masking tape, then fill/overfill with gelcoat. Make sure you put some styrene wax addative in the repair gelcoat and be careful not to use too much catalyst as this could make it porous. Also make sure you remove any air bubbles from the repair gel just by teasing the wet gel repair with a toothpick or similar. Sand and polish.
Fastacraft Facebook page
Reply
Like
8
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
advice on what release to use on pattern berfore laying up mould.
Porkster0
-
10 Years Ago
Hi ian I would try and extend the bonnet scoop pattern edges. Its always better to make the pattern...
scottracing
-
10 Years Ago
I usually release/wax a mould first and then add any yellow wax filling or fillets etc. You can...
Fasta
-
10 Years Ago
Hi Thanks Scottracing and Fasta for the advice. I have created side flanges all around by...
Porkster0
-
10 Years Ago
I always apply release agent before doing the wax to ensure complete coverage, then apply another...
Hanaldo
-
10 Years Ago
Looking good the flange on the back end of the scoop is looking a little small but that could be the...
davro
-
10 Years Ago
HI Hanaldo and Davro Thanks for the advice I will add an extra coat of release now I have done the...
Porkster0
-
10 Years Ago
Hi All Just a quick update have just made and broken out my first mould and must say am very happy...
Porkster0
-
10 Years Ago
Good job and excellent for the first effort. Those damaged edges appear broken away from just...
Fasta
-
10 Years Ago
Post Reply
Like
9
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search