Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Mould Making
»
Alternative moulds
Alternative moulds
Post Reply
Like
3
Alternative moulds
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
111mattin111
111mattin111
posted 9 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 67,
Visits: 910
Hiya when making a mould that I plan on pulling numerous parts from I use the unimould system but on large parts it doesn't work out cheap
Is there a cheaper alternative to making moulds when I only plan on pulling a few parts from it
Paul
Reply
Like
3
panda
panda
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 47,
Visits: 2.1K
You can use standard laminating resin and gelcoat, you just need to ensure you build the mold up slowly and only laminate one layer at a time to stop the heat from building up and distorting it.
www.pandakayaks.co.uk
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search