By 111mattin111 - 5/4/2016 10:20:38 AM

Hiya when making a mould that I plan on pulling numerous parts from I use the unimould system but on large parts it doesn't work out cheap

Is there a cheaper alternative to making moulds when I only plan on pulling a few parts from it

Paul
By panda - 5/4/2016 5:25:56 PM

You can use standard laminating resin and gelcoat, you just need to ensure you build the mold up slowly and only laminate one layer at a time to stop the heat from building up and distorting it.