tiny slits when infusing a flat panel


Author
Message
Davo456
Davo456
Supreme Being (100 reputation)Supreme Being (100 reputation)Supreme Being (100 reputation)Supreme Being (100 reputation)Supreme Being (100 reputation)Supreme Being (100 reputation)Supreme Being (100 reputation)Supreme Being (100 reputation)Supreme Being (100 reputation)
Group: Forum Members
Posts: 8, Visits: 77
Infused a flat panel for the 1st part of my dash, and have got some small slit like marks in the resin.

Unfortunately they don't show up when I photograph them - very small little slits, 5mm long max, and about the width of a letter l.

I'm thinking I didn't shut off resin long enough before the vacuum perhaps ? and they are air bubbles ?

Any ideas ?
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search