I didnt believe this that SHD do glitter preg!!!! but I had someone ask at the JEC Show and they do a glitterpreg! Smile Im going to get some for a gaffer dazzler job at work.
Will get photos of it when it comes in Smile
f1rob
f1rob
Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)
Group: Forum Members
Posts: 237, Visits: 4.8K
Speak to shd you can get some very sparkly pre preg
ChrisR
ChrisR
Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)
Group: Forum Members
Posts: 363, Visits: 3K
Flake looks great when it's done properly but you normally have a solid back colour. If you were infusing you would have to spray in a clear gel, another gel with the flake, then a solid pigmented gel, then layup for infusion.

It's a complete b***h to fix if you ever need to. You also end up having a very thick gelcoat layer which sometimes can crack/craze.
MarkMK
MarkMK
Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)
Group: Forum Members
Posts: 338, Visits: 2K
Has anyone used or experimented with glitter or metal flake-type material when making laminates for added decorative effect?

I'm assuming that it won't penetrate fabric enough to be added to the resin during infusion so perhaps it would need to be added to an in-mould coating or post-production laquer

Bling overkill or can it be done subtley to add a little sparkle to 'plain old carbon'? Smile
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search