Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Mould Making
»
Help please
Help please
Post Reply
Like
10
Help please
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Davidpetty1988
Davidpetty1988
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 26,
Visits: 89
I'm doing a resin infusion so I need a flange all the way around were I have this big gap do I have to just build a wall out of modelling from the base up to the part? I'm using the epoxy tooling gel and putty kit from ec.
Tags
flange
Mould
Reply
Like
10
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Help please
Davidpetty1988
-
10 Years Ago
Hi David, You can just build a wall of modeling plasticine with a layer of filleting wax on the...
davro
-
10 Years Ago
Thanks davro confirmed what I thought it just looks like I made it a lot harder than it should of...
Davidpetty1988
-
10 Years Ago
4 inch flange from the edge of the product to the outside edge of the mould, basically enough space...
davro
-
10 Years Ago
Post Reply
Like
10
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search