Warren (Staff)
Warren (Staff)
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 2.5K,
Visits: 8.5K
Normally we would recommend about 25% pure acetone to thin it down. It may be the 10% you are using isn't enough for the set up you are spraying with.
Start by spraying a 'mist coat' over the pattern. Wait 2-5 minutes for the solvents to evaporate.
Pattern-Coat™ Hi-Gloss can be applied wet-on-wet but sufficient time must be left between passes (2-5 minutes) to allow time for the solvent to evaporate. Around 5 passes should leave a sufficient thickness of Hi-Gloss to ensure the surface can be properly flatted.
Also consider the working temperature and humidity can all play an effect on how it settles on the surface. Even a slight rise in temperature of a few degrees might be enough to change the way it sprays.
For that reason we always recommend working at 20C where possible.
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Reply
Like
7
Hanaldo
Hanaldo
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
Cleaning a HVLP gun is quick and easy too, I've never found cleaning the cup gun to be any easier aside from being able to just throw the cup.
I would recommend getting a cheapish HVLP. I've been using the same one that fibreglast and composite envision sells (around $100) for 2 years spraying all sorts of coatings from 2ks to Duratec to gelcoats. Never had an issue and gives a much more consistent finish off the gun.
Reply
Like
6
67redrocket
67redrocket
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 49,
Visits: 486
I use it because I don't have a spray gun. And the cleaning of the cup gun is fast and easy.
Reply
Like
6
Hanaldo
Hanaldo
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
Why are you spraying it with a cup gun? You would achieve a much better finish using a HVLP spray gun with a 2.5mm tip.
Reply
Like
6
67redrocket
67redrocket
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 49,
Visits: 486
Hello, i have used the hi-gloss pattern coat a while now. I use it with the spray cup gun and a #3 nozzle, and i thin the coat with about 10% acetone
I always get a bad result with lots of tiny high spots. But this morning I got a good result with a flat surface, but I dont understand why.
How do you do it, and what is the best way to apply it with a cup gun?
Reply
Like
6
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
6
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search