Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Resin Infusion
»
Prepping a solid core for infusion
Prepping a solid core for infusion
Post Reply
Like
3
Prepping a solid core for infusion
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
duke
duke
posted 9 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 10,
Visits: 114
I've done some different infusion tests with the 5 and 10 mm PVC foam core.
The 10 mm is the grooved and drilled version and gives an excellet coverage of expoy on the underside of the layup. But on the 5 mm without any grooves or holes the expoy just gets in about 40-50 mm from the outside edges.
I'm about to make large boards with the 5mm. How would you recommend I go about and modify the core to get good coverage?
I'm talking about 4 square meters so e.g. drilling every 25 mm would be preeeetty time consuming.
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Prepping a solid core for infusion
duke
-
9 Years Ago
I would want to be drilling at least every 2 inches to ensure good wet out. I'd probably do 40mm to...
Hanaldo
-
9 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search