Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
Carbon fiber ring
Carbon fiber ring
Post Reply
Like
3
Carbon fiber ring
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
kidpaint
kidpaint
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 99,
Visits: 676
Hey everyone, Its been a while since Ive posted on here. Ive recently got engaged and am wanting to make my own carbon fiber ring. I have a few Ideas on how to go about this but want to hear what others have to say.
On idea it to cut a strip of CF and wet lay it wrapped around a aluminum rod that is machined down to my ring size. That way the inner part matches my finger. Then cut and polish to finish
Another is to buy cf woven tube and do the same principle with the aluminum rod just using this instead.
i just want a nice pattern. nothing fancy inlayed or anything else. Just a nice carbon ring
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Carbon fiber ring
kidpaint
-
10 Years Ago
Calculate your ring size and make or buy some tube.
Fasta
-
10 Years Ago
Hi, I did a few Carbon rings a while back .. I made a very slightly tapering mandrel from...
Dravis
-
10 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search