1st infusion, and it leaked in air
1st infusion, and it leaked in air
Post Reply
Like
3
Prev
1
2
Jump To Page
1st infusion, and it leaked in air
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
LeeBrett
LeeBrett
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 11,
Visits: 167
Yesterdays bagging attempt was much better, until about 45 mins after infusion I thought it would be a good idea to move it onto an electric blanket, then the feed line decided to leak. Oh well another lesson learned.
Nothing good to say......then say nothing
Reply
Like
2
Hanaldo
Hanaldo
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
Yeh, always a risk to move the mould after the infusion. I always cut the hoses off just above the clamp, to limit movement.
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
Prev
1
2
Jump To Page
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search