Group: Forum Members
Posts: 11,
Visits: 167
|
Hi, I just started to practice resin infusion and I made my bag with pleats just like the video tutorials show, I then found a leak on one of the pleats when pulling a vac down and a simple squeeze of the bag tape cured the leak. After a few seconds the gauge went to full vac and the pump noise changed, I then clamped the vac line to do a drop test. returning 20 mins later I noticed that the catch pot lid had leaked and the gauge had dropped so I sealed the lid and then pulled vac on the catch pot up to the line clamp. Then I switched off the pump and opened the clamp to drop test the bag and the gauge stayed the same.
I did the infusion and took it slow and when the resin started going up the catch pot line I clamped off the line followed by the feed line. After returning an hour or so later the bag had lost its vacuum so am I missing something very simple or do I keep scratching my head.
I have no experience of fibreglass or carbon work so I am looking to make mistakes and learn from them before actually taking on the project that I set out to do.
Cheers Lee
Nothing good to say......then say nothing
|