Jacopo Carbonio
Jacopo Carbonio
Supreme Being (343 reputation)Supreme Being (343 reputation)Supreme Being (343 reputation)Supreme Being (343 reputation)Supreme Being (343 reputation)Supreme Being (343 reputation)Supreme Being (343 reputation)Supreme Being (343 reputation)Supreme Being (343 reputation)
Group: Forum Members
Posts: 43, Visits: 109
I think it's only a thin layer of twill (maybe 160gr?) carbon, sprayed with glue before laying, covered with resin and clear coat..nothing so technical Smile
TomDesign
TomDesign
Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)
Group: Forum Members
Posts: 454, Visits: 2.5K
the samw i was thinking only why they use hairdryer?
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
I think it will just be a set-weave carbon with a b-staged epoxy rather than any spray adhesives. Heat guns do give set-weave fabrics a bit more conformability. 
TomDesign
TomDesign
Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)
Group: Forum Members
Posts: 454, Visits: 2.5K
any link of this carbon?
a set-weave carbon with a b-staged epoxy
Fasta
Fasta
Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
Looks like everyday 200g dry twill carbon, stuck down with some adhesive and wet out like many do with wrapping parts.

Maybe the hairdryer is just meant to confuse us? 

Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
TomDesign (12/12/2015)
any link of this carbon?
a set-weave carbon with a b-staged epoxy


Fasta
Fasta
Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
Hanaldo (12/12/2015)
TomDesign (12/12/2015)
any link of this carbon?
a set-weave carbon with a b-staged epoxy


EC's Profinish carbon is one example of such a fabric.



This type of carbon is just dry carbon with a binder sprayed on one side to hold the weave from distorting too easy.  Just another style of dry carbon. 

What's the hairdryer for?




Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Yes, that's all a set-weave carbon is. It's just a dry fabric, with a binder sprayed on it as you said. The binder is a polymer, and is often a b-staged epoxy. I'm sure I remember Paul saying when I was in England that the Profinish fabric uses an epoxy binder, but I could be remembering a different product. 

That's what I was getting at with my original reply. I think the fabric being used in that video is simply a set-weave dry carbon fabric. These fabrics lose quite a lot of their drape and conformability because of the binder stopping the fibres from moving, but if you warm them up with a hair dryer then the binder loosens up a bit. It's very much like a pre-preg fabric, it's just partially impregnated. 
TomDesign
TomDesign
Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)
Group: Forum Members
Posts: 454, Visits: 2.5K
yes but with hair dryer it losses stable but how it looks like used like epoxy after tacky time to put on but on video he put on soft surface )