Will try resin infusion for The first time tomorrow. What is The ideal temperature for This, i Will be using easy composites infusion epoxy.




I see that some on This forum is covering The mould With blanckets and heating it up. What is The purpose og This?
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Ideal temp is 25 degrees. Anywhere between 18-30 degrees is fine. Any colder than that and you will want to warm up your resin and mould (hence the blankets). Any hotter and you'll want to keep an eye on your resins exotherm, don't mix large batches or you could get stuck with a bit of a mess! 
VVS
VVS
Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)
Group: Moderators
Posts: 226, Visits: 334
I'm using a three setting heated electric blanket and an old duvet to keep a steady temperature as my work area is not heated at night.

once covered the infusion stays warm with the blanket set to low heat so a nice cheap and simple way of curing small parts.