By 67redrocket - 10/8/2015 12:34:05 PM
Will try resin infusion for The first time tomorrow. What is The ideal temperature for This, i Will be using easy composites infusion epoxy.
I see that some on This forum is covering The mould With blanckets and heating it up. What is The purpose og This?
|
By VVS - 10/8/2015 9:41:10 PM
I'm using a three setting heated electric blanket and an old duvet to keep a steady temperature as my work area is not heated at night.
once covered the infusion stays warm with the blanket set to low heat so a nice cheap and simple way of curing small parts.
|
|