First part: Interior panel


Author
Message
67redrocket
67redrocket
Supreme Being (697 reputation)Supreme Being (697 reputation)Supreme Being (697 reputation)Supreme Being (697 reputation)Supreme Being (697 reputation)Supreme Being (697 reputation)Supreme Being (697 reputation)Supreme Being (697 reputation)Supreme Being (697 reputation)
Group: Forum Members
Posts: 49, Visits: 486
Hello I'am going to start up with my first carbon fiber part. Its a small interior panel. As this is my first part I want some help so I don't do too many mistakes in the beginning. I have bought some chemicals for the mold that I'am going to pick up saturday:

Epoxy Tooling Gelcoat
Easy-Lease Chemical Release Agent1
Epoxy Mould Making Putty
Soft Filleting and Filling Wax
Meguiar's mirror glaze mold release wax nr. 8

I have attached a picture of the panel I want to create a mould from. Its steel and the bondo is a polyester body bondo. 

For the  flanges arround the part I have bought polypropylene sheets as I have read that the gelcoat would not stick to the PP plastic. 

I am wondering if i should wax the part before I apply the Easy-lease, or should I use Easy-lease before I wax the part???

http://www.talkcomposites.com/Uploads/Images/61e49fd3-aca3-4705-a622-7a34.jpg
Hanaldo
Hanaldo
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Always Easy-lease BEFORE waxing the part! 
67redrocket
67redrocket
Supreme Being (697 reputation)Supreme Being (697 reputation)Supreme Being (697 reputation)Supreme Being (697 reputation)Supreme Being (697 reputation)Supreme Being (697 reputation)Supreme Being (697 reputation)Supreme Being (697 reputation)Supreme Being (697 reputation)
Group: Forum Members
Posts: 49, Visits: 486
Thank you Hanaldo

I picked up the mold equipment on saturday, but I was not satisfied with the surface after sanding the bondo. The panel was straight but there was small holes in the bondo. So I had to apply a spray can bondo that i got from a friend yesterday. Is the easycomposites Pattern-Coat Hi-Gloss better to use after i got the plug straight? 

How do I get the best surface on a plug I want high gloss?

Iam going to sand it down today and hopefully start making the mold. 
Hanaldo
Hanaldo
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Yeh body filler tends to end up pretty porous, one normally seals it with a spray filler. 

The high gloss pattern coat would give you a great finish, unfortunately you might run into problems having now sprayed it with a single pack aerosol. 
carbonfibreworks
carbonfibreworks
Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)
Group: Forum Members
Posts: 292, Visits: 4.5K
Hi Redrocket
Only one way forward with this and its quick and easy use PVA release, you will have a bit of polishing to do on the mould but a guaranteed release.
Regards Chris

http://www.talkcomposites.com/Uploads/Images/97e08777-693c-4af1-a27a-86cf.png
Edited 11 Years Ago by carbonfibreworks
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search