Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
From a structural perspective, glass fibre is fine for skinning but not as high a performance material as carbon fibre.
Corrosion between conductive metals can be prevented with a thin layer of glass fibre or resin between the two metals.