Group: Forum Members
Posts: 1,
Visits: 7
|
Am very interested in this also, and been looking at using the Braided Sleeve to make the tube. Issue that's got me though is bending it to make say an S bend or something. The silicone hose sounds good, but in a case like an S shaped tube getting it out could be an issue no? or just really polish it up first? or is there possibly some polyuathane rode which could be use in it and dissolved out later as an idea? But am very interested in knowing a good solution to this other than a two part mould which would be bit overkill for what I'm trying to fashion.
|