Hi guys,
Is there any body can give me some idea how to make a carbon fibre tube?
what process can be reliable to make carbon fibre tube?
How to build the mould for the tube?
Looking forward to your advice
Leon
By CarbonMike
-
12/27/2012 10:03:25 PM
You could quite easily use a vac bag inside a two piece mould to make a tube. Then envelope bag the entire mould and vac it.