Here's a few more pics.

 

First off hear is the engine covers de-moulded. They came out good, except the large one has a Piece of carbon floating in there. I am going to make a pattern and pre cut every piece from now on.

http://www.carbontuner.com/talk/7-5-12/engine1.png
http://www.carbontuner.com/talk/7-5-12/engine2.png


I plan to just leave these parts bare carbon and sell them cheap to someone local. My car has a Super Charge on it now so the rear plate wont even fit. I found a guy in indonesia whom is sending me his elise SC engine cove which I think will fit mine too. So I will make his and mine, then send him his Part in CF and his orginal for free, Hope I don't break his part. I only broke one but I am pretty confident now. Now the biggest demould problem is some painted parts are reacting to this orange tooling gel I am using and blisters the paint occasionally. fortunately for me the part at hand is not painted, just abs plastic.

 

Another project up next is making the side scoop molds for my elise. I actually bought a set of CF ones before I got into making the parts. Still I need the mould to add the part to my online store + I may use a hybrid red/black fabric for the outer layer.

http://www.carbontuner.com/talk/7-5-12/scoop.png



If Brute Force Isn''''t working your not using enough...
Carbon Tuner
Carbon Tuner
Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)
Group: Forum Members
Posts: 104, Visits: 422
Some More pics. I have the door pulls mastered. Also Get to se a plain weave version of the engine cover. Got a 2x2 set on the way. Will pop out of mold tommorow. This is the first piece out of the larger mold cant wait to see it!

 

http://www.carbontuner.com/talk/jun12/cover.png

http://www.carbontuner.com/talk/jun12/mold.png

Door pulls

http://www.carbontuner.com/talk/jun12/pull.png

http://www.carbontuner.com/talk/jun12/pull2.png

http://www.carbontuner.com/talk/jun12/pull.png



If Brute Force Isn''''t working your not using enough...
Dave
Dave
Supreme Being (478 reputation)Supreme Being (478 reputation)Supreme Being (478 reputation)Supreme Being (478 reputation)Supreme Being (478 reputation)Supreme Being (478 reputation)Supreme Being (478 reputation)Supreme Being (478 reputation)Supreme Being (478 reputation)
Group: Forum Members
Posts: 48, Visits: 253
Great Stuff, can't wait to see the intake cover!w00t

Dave.
pk_090
pk_090
Supreme Being (383 reputation)Supreme Being (383 reputation)Supreme Being (383 reputation)Supreme Being (383 reputation)Supreme Being (383 reputation)Supreme Being (383 reputation)Supreme Being (383 reputation)Supreme Being (383 reputation)Supreme Being (383 reputation)
Group: Forum Members
Posts: 47, Visits: 169
That looks awesome! is that a big sheet of perspex you are moulding on in the first pic?
Alex
Carbon Tuner
Carbon Tuner
Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)
Group: Forum Members
Posts: 104, Visits: 422
O here's some images of me making my parts, Ill update this thread more when I get the orginal parts out of the mold or make the cf ones. these parts are for a 2006 lotus elise s2 Federal

This is the 4th attempt at this mold.... I have bean trying to get these door pulls during my whole learning process. first one I made was good but I forgot to put pva and wax on it before making my part... second one had thin spots third leaked now this....

http://www.carbontuner.com/talk/61312/mold.png

Here's the door puls finished this one mold I am making will be the final mold, I made this one in the photo with a leaky mold, so after the part came out I pitched it again...

http://www.carbontuner.com/talk/61312/pulls.png

Acess panel covers... I threw away these molds once because I thought it would be slick to put a few 45 degree angles in the corners of the mold face, tell I tried to bag that with pleats lol..

http://www.carbontuner.com/talk/61312/mol.png

Some finished products made with old molds, this one above was 1 of 2 pressure tested 24 hrs, ready to get the best polish I ever did!


Attempt 1 cleared and polished!
http://www.carbontuner.com/talk/61312/cover.png

I clear coated this then sanded to 500, still waiting finish up..


attempt 2!
http://www.carbontuner.com/talk/61312/matte.png

Here's a spark plug cover that was from again a leaky mold, but I made all these molds before I knew to watch for debris like a hawk...

http://www.carbontuner.com/talk/61312/spark.png

Here's the new mold and the intake cover in process too:

http://www.carbontuner.com/talk/61312/mold2.png

Annnnnd here's the next 2 target pieces. Yes what you see now is what I like to cal "Farbon Fiber"

http://www.carbontuner.com/talk/61312/car.png



If Brute Force Isn''''t working your not using enough...
Edited 13 Years Ago by Carbon Tuner
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search