Hi,

I would like to make a small straight razor blade (so size is 14 X 2 cm max.)
I would like to make it in a closed mould under high pressure (so it made of 1piece).
I want to have the carbon cosmetic finish on both sides so here is my issue.
All infusion I saw had one flat surface on the side of the bagging.
If I do not use peel-ply and / or infusion mesh is it possible to succeed with infusion if the part is very small?
If I use Easy Lease knitted mesh does it make a difference?
How can I get 2 cosmetic sides on my razor blade?

Thanks for your help.
Kind Regards,
Olivier
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search