Machining of polyurethane board


Author
Message
JB
JB
JB
posted 14 Years Ago HOT
Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)
Group: Forum Members
Posts: 1, Visits: 4
We have a request to machine medium and high density polyurethane boards from easycomposites (for a student's project) on a CNC milling machine.  Are there any ready tables of recommeded type of cutters, cutting method (wet or dry), feeds, cutting speed, ect.  Support is appreciated. Thanks