We have a request to machine medium and high density polyurethane boards from easycomposites (for a student's project) on a CNC milling machine.  Are there any ready tables of recommeded type of cutters, cutting method (wet or dry), feeds, cutting speed, ect.  Support is appreciated. Thanks
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Hi JB,

Thanks for the post. I think I've spoken to you about this on phone.

The PU foams and tooling boards don't really come with any recommended cutting settings for CNC machining. They are of course intended specifically for the purpose (the model boards particularly) and so should machine really well. In general terms, you could use bits and speeds appropriate for MDF on the medium density modelboard and high density modelboards and even faster cutting speeds for the foams which will really present very little resistance to the router.

I hope this helps.

Best regards, Matt

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search