Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Easy Composites Ltd Technical Support
»
Easy Composites Ltd - General Technical Support
»
uni mould system.../ mould release compatibility
uni mould system.../ mould release compatibility
Post Reply
Like
9
uni mould system.../ mould release compatibility
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
ARSOUILLERB26
ARSOUILLERB26
posted 14 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 16,
Visits: 122
Hi everyone
Like you imagine, I need help about a few questions, I ll try to be short:
1) My first question is about the uni mould making system:
I saw it's cheaper than epoxy mould systems, with high compatibility with epoxy and polyester (perfect for sticky spray).
So that is for the pros but does it exist cons?
Because if not, I will make each mould (big or not) with that system instead of epoxy.
2) I would like to know if it exist compatibility problems between the differents release systems (PVA, chemical or wax)?
For exemple, can I use the chemical release agent on a mould witch was waxed several times before?
Does the mould cleaner destroy the pva, was or chemical release barieer?
3) I discovered your sticky spray on your tutorial witch looked awesome to keep layers in place before the infusion (a real problem for me) but actually, all my moulds was made with epoxy gel coat (I saw it cannot be used with)...
HAve you a solution for me? And when will it be available on you shop
?
thank you by advance for your answers
cheers
Reply
Like
9
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
uni mould system.../ mould release compatibility
ARSOUILLERB26
-
14 Years Ago
Hi, Sorry for the delay in getting back to you; answers to your questions as follows: [quote] 1)...
Matt (Staff)
-
14 Years Ago
No problem for the delay matt, really glad to read you. 1) the smell is not a problem for me, I...
ARSOUILLERB26
-
14 Years Ago
Hi, You're welcome. Answers as follows: [quote]But what to you mean about "high pressure...
Matt (Staff)
-
14 Years Ago
Or you could take a look at this spray tack... 3M™ Adjustable Composite Positioning System...
Kevin-Lee
-
14 Years Ago
Has anyone found this product in europe? [quote][b]Kevin-Lee (16/06/2012)[/b][hr]Or you could take...
prsw
-
13 Years Ago
thank you for all that very accurate explanations matt, I tried the stay z yesterday: very usefull....
ARSOUILLERB26
-
14 Years Ago
We haven't been able to source it either. It seems they have released the product then it's...
Warren (Staff)
-
13 Years Ago
I have asked 3M Sweden but only got an answer that the product is not available in Sweden....
prsw
-
13 Years Ago
Post Reply
Like
9
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search