Hi everyone Smile

Like you imagine, I need help about a few questions, I ll try to be short:


1)  My first question is about the uni mould making system:
I saw it's cheaper than epoxy mould systems, with high compatibility with epoxy and polyester (perfect for sticky spray).
So that is for the pros but does it exist cons?
Because if not, I will make each mould (big or not) with that system instead of epoxy. BigGrin


2)   I would like to know if it exist compatibility problems between the differents release systems (PVA, chemical or wax)?
For exemple, can I use the chemical release agent on a mould witch was waxed several times before?
Does the mould cleaner destroy the pva, was or chemical release barieer?


3)   I discovered your sticky spray on your tutorial witch looked awesome to keep layers in place before the infusion (a real problem for me) but actually, all my moulds was made with epoxy gel coat (I saw it cannot be used with)... Ermm
HAve you a solution for me? And when will it be available on you shop Wink?

thank you by advance for your answers BigGrin

cheers



Replies
Kevin-Lee
Kevin-Lee
Supreme Being (376 reputation)Supreme Being (376 reputation)Supreme Being (376 reputation)Supreme Being (376 reputation)Supreme Being (376 reputation)Supreme Being (376 reputation)Supreme Being (376 reputation)Supreme Being (376 reputation)Supreme Being (376 reputation)
Group: Forum Members
Posts: 44, Visits: 2.4K
Or you could take a look at this spray tack...

3M™ Adjustable Composite Positioning System 11095.

3M ACPS 11095.

http://a248.e.akamai.net/origin-cdn.volusion.com/3oysk.639mx/v/vspfiles/photos/70006732021-2.jpg?1337206575

..."
3M introduces the new 3M(TM) Adjustable Composite Positioning System (ACPS) 11095, an easy-to-use positioning spray designed for pre-infusion resin bond dry reinforcements and composite matrices. The unique properties of 3M ACPS 11095 enable it to integrate into the part during resin infusion, eliminating read-through and transition layers in the part post-cure. This patent-pending system offers manufacturers benefits in productivity, esthetics and flexibility. 3M ACPS 11095 is uniquely formulated to be compatible with most resin systems, including polyester, vinyl ester and epoxy resins. It goes down easily on both flat and curved mold designs, and after spraying, the product builds tack within seconds and is tack-free in two to three minutes. Designed with ease-of-use in mind, the product features a unique color change system that gives it a blue color when first sprayed, then fades to clear as it cures. With this feature, users can easily see the amount of coverage they've achieved, and also have a visual indication of the curing cycle. 3M ACPS 11095 is not affected by ambient temperature and/or humidity, allowing it to be used in a variety of manufacturing conditions.

Additional user-friendly features of 3M ACPS 11095 allow substrates to be easily repositioned without leaving fibers behind, simply by peeling back an individual layer and reapplying. If the coating dries before laying up of materials, an additional coating can be applied at a lower rate, which reactivates the previously applied coating. The product also enables manufacturers to use less than competitive brands.

3M ACPS 11095 has the ability to hold most types of reinforcement and to maintain the position of reinforcement for days without sagging. With typical usage, users will see little to no change in laminate shear properties. Available in aerosol cans as well as five-gallon and 55-gallon containers compatible with most traditional spray equipment, the product is also easy to clean up with most solvents. 3M ACPS 11095 is approved by Lloyd's Register and DNV"...

Cheers,

Kev.
Edited 14 Years Ago by Kevin-Lee
prsw
prsw
Supreme Being (908 reputation)Supreme Being (908 reputation)Supreme Being (908 reputation)Supreme Being (908 reputation)Supreme Being (908 reputation)Supreme Being (908 reputation)Supreme Being (908 reputation)Supreme Being (908 reputation)Supreme Being (908 reputation)
Group: Forum Members
Posts: 112, Visits: 1K
Has anyone found this product in europe?


Kevin-Lee (16/06/2012)
Or you could take a look at this spray tack...

3M™ Adjustable Composite Positioning System 11095.

3M ACPS 11095.

http://a248.e.akamai.net/origin-cdn.volusion.com/3oysk.639mx/v/vspfiles/photos/70006732021-2.jpg?1337206575

..."
3M introduces the new 3M(TM) Adjustable Composite Positioning System (ACPS) 11095, an easy-to-use positioning spray designed for pre-infusion resin bond dry reinforcements and composite matrices. The unique properties of 3M ACPS 11095 enable it to integrate into the part during resin infusion, eliminating read-through and transition layers in the part post-cure. This patent-pending system offers manufacturers benefits in productivity, esthetics and flexibility. 3M ACPS 11095 is uniquely formulated to be compatible with most resin systems, including polyester, vinyl ester and epoxy resins. It goes down easily on both flat and curved mold designs, and after spraying, the product builds tack within seconds and is tack-free in two to three minutes. Designed with ease-of-use in mind, the product features a unique color change system that gives it a blue color when first sprayed, then fades to clear as it cures. With this feature, users can easily see the amount of coverage they've achieved, and also have a visual indication of the curing cycle. 3M ACPS 11095 is not affected by ambient temperature and/or humidity, allowing it to be used in a variety of manufacturing conditions.

Additional user-friendly features of 3M ACPS 11095 allow substrates to be easily repositioned without leaving fibers behind, simply by peeling back an individual layer and reapplying. If the coating dries before laying up of materials, an additional coating can be applied at a lower rate, which reactivates the previously applied coating. The product also enables manufacturers to use less than competitive brands.

3M ACPS 11095 has the ability to hold most types of reinforcement and to maintain the position of reinforcement for days without sagging. With typical usage, users will see little to no change in laminate shear properties. Available in aerosol cans as well as five-gallon and 55-gallon containers compatible with most traditional spray equipment, the product is also easy to clean up with most solvents. 3M ACPS 11095 is approved by Lloyd's Register and DNV"...

Cheers,

Kev.



http://motoform.blogspot.se

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search