Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
Shear test for chopped strand mat (CSM)
Shear test for chopped strand mat (CSM)
Post Reply
Like
3
Shear test for chopped strand mat (CSM)
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Fateme
Fateme
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 2,
Visits: 8
Hello everybody
I want to define mechanical properties for Chopped Strand Mat (CSM) composite material,
But I have a problem with the shear test; CSM has random- discontinuous fibers and I don't know how to cut the specimen in _+45 for shear test.
Is it similar to tensile specimens?
Thanks in advanced
Reply
Like
3
ChrisR
ChrisR
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 363,
Visits: 3K
It shouldn't matter
Reply
Like
2
Fateme
Fateme
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2,
Visits: 8
Thanks ChrisR
So how many layers should be used for the shear test specimens?
ASTM d3518 has some notes for the number of the layers of WR and unidirectional, and there is no any thing for CSM.
Reply
Like
3
ChrisR
ChrisR
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 363,
Visits: 3K
That's up to you isn't it!
It will depend on what you are comparing it to and the weight of CSM you are using! 2 layers of 0.3oz will be a lot thinner then 2 layers of 9oz !
Reply
Like
2
Hanaldo
Hanaldo
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
Are you trying to obtain a value that you can express in units, or a value relative to another material?
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search