Resin


Author
Message
Shaneer22
Shaneer22
Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)
Group: Forum Members
Posts: 156, Visits: 14K
Does anyone no where I stand I bought resin and hardener not from easy composites,I infused my part but have just noticed that I was supplied with wrong harderner I think part is screwed,would it be the suppliers fault,I asked for resin and appropriate harderner.if part is screwed would they be responsible for materials as well.