By Shaneer22 - 3/23/2015 10:40:19 PM

Does anyone no where I stand I bought resin and hardener not from easy composites,I infused my part but have just noticed that I was supplied with wrong harderner I think part is screwed,would it be the suppliers fault,I asked for resin and appropriate harderner.if part is screwed would they be responsible for materials as well.
By Shaneer22 - 3/24/2015 2:33:23 PM

Spoke to them today they did give me wrong harderner for this resin system,they want me to post cure them give. Them a sample of resin which I had left over,then they will test it to see if the part can be saved,given them a chance.