Does anyone no where I stand I bought resin and hardener not from easy composites,I infused my part but have just noticed that I was supplied with wrong harderner I think part is screwed,would it be the suppliers fault,I asked for resin and appropriate harderner.if part is screwed would they be responsible for materials as well.
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
You're asking the wrong people if it wasn't from EC, go and talk to the supplier about it. Either they will be apologetic and replace your resin and maybe your materials, or they won't. And if you really feel like you've been wronged and it is worth the effort, then you might take the appropriate legal action. 

End of the day, you have to weigh up how much you have really lost. It happened to me once where my supplier mixed up my hardener and it stuffed up one of my parts. They replaced the resin for me, but I didn't push it harder as I have a good relationship with my supplier. 
ChrisR
ChrisR
Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)
Group: Forum Members
Posts: 363, Visits: 3K
When you say wrong hardener, what exactly is wrong about it? - It may be a different hardener than you usually have but may be OK with certain cure conditions?

Post up the data sheets for the resin & hardener
Shaneer22
Shaneer22
Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)
Group: Forum Members
Posts: 156, Visits: 14K
Spoke to them today they did give me wrong harderner for this resin system,they want me to post cure them give. Them a sample of resin which I had left over,then they will test it to see if the part can be saved,given them a chance.