Hi,

I have question about pre-peg.

1) If I dont have special oven or autoclave I can made items from pre-peg carbon fiber?


Example...

2) I made mold.... Than I use pre-peg carbon fiber +  vacuum bag/ pump and wait 2 days...

What happening? I can made something if I use this strategy? Or I need obligatory warming pre-peg?


3) I can use kitchen electric oven? Something like this...

http://www.rdveikals.lv/images/full/9f7b92e2385550cd3c8c2bc6d64769a8.jpg

 I only need made hole for vacuum pump. Right?


Soory about my english skill.
Thanks.