Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Resin Infusion
»
Producing an octagon shape with RI?
Producing an octagon shape with RI?
Post Reply
Like
3
Producing an octagon shape with RI?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Bbruce99
Bbruce99
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 3,
Visits: 16
Good afternoon folks,
Just thought I would pop in and say hello, and ask a quick question
I am currently building a large telescope from scratch and have been looking at different methods of creating the structure, one of which is a resin infused laminate.
I have attached an image of the part I want to produce, the overall diameter of the exterior diameter is about 14 inches. The smaller holes have been designed out so it is a solid piece with the large hole in the centre. The part will be 10mm thick. I am using roving mat and a 3d core material.
Would resin infusion work with this shape? I was planning on running spiral coil around half of the exterior circumference and drawing the vacuum from the opposite side.
My concern is the resin will not penetrate the depth of the laminate, would it be better to laminate two halves and then bond them together?
Any assistance would be greatly appreciated!
B.
Attachments
image.jpg
(
510 views,
63.00 KB
)
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Producing an octagon shape with RI?
Bbruce99
-
11 Years Ago
I can't see why infusion wouldn't work for that. If it was a 10mm thick laminate then you might have...
Hanaldo
-
11 Years Ago
That's great - thanks for the pointers, I shall let you know how I get on
Bbruce99
-
11 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search