Producing an octagon shape with RI?


Author
Message
Bbruce99
Bbruce99
Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)
Group: Forum Members
Posts: 3, Visits: 16
That's great - thanks for the pointers, I shall let you know how I get on 
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
I can't see why infusion wouldn't work for that. If it was a 10mm thick laminate then you might have issues, but with PET infusion core you'll be fine. The better way to plumb your resin and vacuum lines would be to have the resin feed in the middle and the vacuum spiral around the outer circumference to infuse evenly from the middle. 
Bbruce99
Bbruce99
Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)
Group: Forum Members
Posts: 3, Visits: 16
Good afternoon folks,

Just thought I would pop in and say hello, and ask a quick question 

I am currently building a large telescope from scratch and have been looking at different methods of creating the structure, one of which is a resin infused laminate. 
I have attached an image of the part I want to produce, the overall diameter of the exterior diameter is about 14 inches.  The smaller holes have been designed out so it is a solid piece with the large hole in the centre.  The part will be 10mm thick.  I am using roving mat and a 3d core material.
Would resin infusion work with this shape? I was planning on running spiral coil around half of the exterior circumference and drawing the vacuum from the opposite side.  
My concern is the resin will not penetrate the depth of the laminate, would it be better to laminate two halves and then bond them together?

Any assistance would be greatly appreciated!

B.
Attachments
image.jpg (500 views, 63.00 KB)
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search